Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0130 g/cc | >= 0.000470 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0130 - 1.18 g/cc | 0.000470 - 0.0426 lb/in³ | Average value: 0.974 g/cc Grade Count:117 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Density | >= 0.0130 g/cc | >= 0.000470 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova T443C Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us.. |
|||
Density | 0.0130 - 0.0250 g/cc | 0.000470 - 0.000903 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.0130 - 0.0140 g/cc | 0.000470 - 0.000506 lb/in³ | |
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure.. |
|||
Density | 0.0130 - 0.0140 g/cc | 0.000470 - 0.000506 lb/in³ | |
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Density | 0.0130 g/cc | 0.000470 lb/in³ | Based on 80 times expansion |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Density | 0.0130 g/cc | 0.000470 lb/in³ | Based on 80 times expansion |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Density | 0.0130 - 0.0300 g/cc | 0.000470 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® IA 3000 Expandable Polystyrene, Special Purpose
(discontinued **) Particle size range is 0.7 - 0.9 mm. Minimum apparent density after two expansions is 12 g/l. Minimum apparent density on a discontinuous pre-expander is 14 g/l.Processing technology used for Type .. |