Thermoplastic
Polyetherimide (PEI)
Polyetherimide (PEI), Glass + Carbon Fiber Filled
Category :
Polyetherimide (PEI), Glass + Carbon Fiber Filled
Product List
Tips:
Max 50 items displayed. For more, contact customer service.
PRODUCT NO.
Manufacturer
Trade Name
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced (discontinued **)
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced (discontinued **)