Category Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler , Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler , Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler , Polyphenylene Sulfide (PPS) with 60% Glass Fiber Filler
Manufacturer Celanese Corporation
Tips: 50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category
Celanese FORTRON 4665B6 PPS, 65% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6150T6 PPS, 50% Reinforcement  (Unverified Data**) Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Celanese FORTRON 6160B4 PPS, 60% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6165A4 PPS, 65% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6165A6 PPS, 65% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6341L4 PPS, 40% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 6345L4 PPS, 30% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Celanese FORTRON 6850L6 PPS, 50% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON CES50 PPS, 40% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON FX4382T1 PPS, Impact Modified  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON ICE 504L PPS, 40% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON ICE 506L PPS, 40% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON ICE 716A PPS, 65% Mineral / Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 0205B4/20µm PPS, Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON 214 PPS  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON 309 PPS  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON 320 PPS  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON 1115L0 PPS, 15% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Celanese FORTRON 1120L4 PPS, 20% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Celanese FORTRON 1131L4 ITT PPS, 30% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1200L1 PPS, Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS)
Celanese FORTRON 1342L4 PPS, 40% Specialty  (Unverified Data**) Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1115L0 PPS, 15% Specialty Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Celanese FORTRON 1120L4 PPS, 20% Specialty Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Celanese FORTRON 1131L4 ITT PPS, 30% Glass Reinforced Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140LC6 PPS, 40% Specialty Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1342L4 PPS, 40% Specialty Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 309 PPS, Unfilled Polyphenylene Sulfide (PPS)
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 4184L6 PPS, 53% Mineral / Glass Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6150T6 PPS, 50% Specialty Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Celanese FORTRON 6160B4 PPS, 60% Mineral / Glass Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6162A7 PPS, Mineral / Glass Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON 6165A4 PPS, 65% Mineral / Glass Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese FORTRON MT9141L4 DW PPS, 40% Specialty Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON MT9203HS PPS, Medical Technology Polyphenylene Sulfide (PPS)
Celanese FORTRON 0203HS PPS, Unfilled Polyphenylene Sulfide (PPS)
Celanese FORTRON 0205B4/20µm PPS, Specialty Polyphenylene Sulfide (PPS)
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 1141L4 PPS, 40% Glass Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler