Celanese Celcon® GB10 POM, 10% Glass Reinforced Acetal Copolymer, 10% Glass Fiber Reinforced
Celanese Celcon® GB25 POM, 25% Glass Reinforced Acetal Copolymer, 30% Glass Fiber Reinforced
Celanese Celcon® GC15 POM, 15% Glass Reinforced Acetal Copolymer, 20% Glass Fiber Reinforced
Celanese Celcon® GC25TF POM, 25% Glass Reinforced Acetal Copolymer, 30% Glass Fiber Reinforced
Celanese Celcon® GC90UV POM, 10% UV Resistant Acetal Copolymer, 10% Glass Fiber Reinforced
Celanese Celcon® LU02 POM, UV Resistant Acetal (POM)
Celanese Celcon® M90-45XAP® POM, Specialty Acetal (POM)
Celanese Celcon® M90-45H POM, UV Resistant Acetal (POM)
Celanese Celcon® M90SW POM, Tribological Acetal (POM)
Celanese Celcon® M90UV POM, UV Resistant Acetal (POM)
Celanese Celcon® MC90 POM, Mineral Reinforced Acetal Copolymer, Mineral Filled
Celanese Celcon® MR50B POM, Specialty Acetal (POM)
Celanese Celcon® UV140LG POM, UV Resistant Acetal (POM)
Celanese Celcon® UV270Z POM, UV Resistant Acetal (POM)
Celanese Celcon® WR25Z POM, UV Resistant Acetal (POM)
Celanese Celcon® WR90Z POM, UV Resistant Acetal (POM)
Celanese Celcon® CF802 POM, Specialty Acetal (POM)
Celanese Celcon® GC10 POM, 10% Glass Reinforced Acetal Copolymer, 10% Glass Fiber Reinforced
Celanese Celcon® GC20 POM, 20% Glass Reinforced Acetal Copolymer, 20% Glass Fiber Reinforced
Celanese Celcon® GC25A POM, 25% Glass Reinforced Acetal Copolymer, 30% Glass Fiber Reinforced
Celanese Celcon® LM90Z POM, Specialty Acetal (POM)
Celanese Celcon® LW90 POM, Tribological Acetal (POM)
Celanese Celcon® LW90-S2 POM, Tribological Acetal (POM)
Celanese Celcon® LW90-SC POM, Tribological Acetal (POM)
Celanese Celcon® M140 POM, Unfilled Acetal (POM)
Celanese Celcon® M140-L1 POM, Tribological Acetal (POM)
Celanese Celcon® M15HP POM, Unfilled Acetal (POM)
Celanese Celcon® M25 POM, Unfilled Acetal (POM)
Celanese Celcon® M25UV POM, UV Resistant Acetal (POM)
Celanese Celcon® M270™ POM, Unfilled Acetal (POM)
Celanese Celcon® M270UV POM, UV Resistant Acetal (POM)
Celanese Celcon® M450 POM, Unfilled Acetal (POM)
Celanese Celcon® M50 POM, Unfilled Acetal (POM)
Celanese Celcon® M90-07 POM, Color Concentrate Acetal Copolymer, Unreinforced
Celanese Celcon® M90-34 POM, Unfilled Acetal (POM)
Celanese Celcon® M90LF POM, Unfilled Acetal (POM)
Celanese Celcon® M90™ POM, Unfilled Acetal (POM)
Celanese Celcon® MR25B POM, Specialty Acetal (POM)
Celanese Celcon® MR90B POM, Specialty Acetal (POM)
Celanese Celcon® UV25Z POM, UV Resistant Acetal (POM)
Celanese Celcon® UV90Z POM, UV Resistant Acetal (POM)
Celanese Celcon® LW25-S2 POM, Tribological Acetal (POM)
Celanese Celcon® LW90-F2 POM, Tribological Acetal (POM)
Celanese Celcon® GC25T POM, 25% Glass Reinforced Acetal Copolymer, 30% Glass Fiber Reinforced
Celanese Celcon® LW90FS-K POM, Tribological Acetal (POM)
Celanese Celcon® M90AW POM, Tribological Acetal (POM)
Celanese Celcon® MC270 POM, Mineral Reinforced Acetal Copolymer, Mineral Filled
Celanese Celcon® MC270-HM POM, Mineral Reinforced Acetal Copolymer, Mineral Filled
Celanese Celcon® MC90-HM POM, Mineral Reinforced Acetal Copolymer, Mineral Filled
Copyright © lookpolymers.com All Rights Reserved