Material Notes:
Neoplast 163 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
ASTM D 2240
68

@Time 605000 sec
68

@Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 6.77 MPa
981 psi
500 mm/min; ASTM D 412
7.45 MPa

@Time 605000 sec
1080 psi

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 425 %
425 %
500 mm/min; ASTM D 412
361 %

@Time 605000 sec
361 %

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00539 GPa
0.782 ksi
500 mm/min; ASTM D 412
Tear Strength 21.6 kN/m
123 pli
500 mm/min; ASTM D 624
Compression Set 28 %

@Temperature 70.0 °C,
Time 79200 sec
28 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuous; SAE J 2236
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D 746