Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP)
Manufacturer Zylog Plastalloys
Trade Name Hipolyene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Melt Flow 9.0 g/10 min
9.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.6 MPa
3270 psi
Elongation at Break 75 %
75 %
Flexural Modulus 2.21 GPa
320 ksi
Izod Impact, Notched 1.77 J/cm
3.31 ft-lb/in