Material Notes:
Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.This grade is ideal for soft trim in combination with leathers, textiles and decorative laminates, including low FST cores for composites and divider panels.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0740 g/cc
0.00267 lb/in³
ISO 845
Mechanical Properties Metric English Comments
Tensile Strength 1.00 MPa
145 psi
ISO 1798
Elongation at Break 90 %
90 %
Compressive Yield Strength 0.150 MPa

@Strain 25.0 %
21.8 psi

@Strain 25.0 %
ISO 7214
Compression Set 20 %

@Time 79200 sec,
Strain 50.0 %
20 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ISO 7214
Thermal Properties Metric English Comments
Thermal Conductivity 0.0323 W/m-K
0.224 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0369 W/m-K
0.256 BTU-in/hr-ft²-°F
mean temp of 50°C; ISO 8301
0.0416 W/m-K
0.289 BTU-in/hr-ft²-°F
mean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 157 °C
315 °F
Descriptive Properties Value Comments
Flammability Heat Release: FAR/CS 25.853, 2 min total
Pass at 13 mm
Heat Release: FAR/CS 25.853, Peak
Pass at 13 mm
Radiant Heat Panel: FAR 25.856
Pass at 3, 13, and 25 mm
Smoke Density: ABD0031
Pass at 13 mm
Smoke Density: FAR/CS 25.853
Pass at 13 mm
Toxic Gas Emission: ABD0031
Pass at 13 mm
Vertical Burner (60 sec): FAR/CS 25.853
Pass at 25 mm