Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0850 - 0.130 g/cc
0.00307 - 0.00470 lb/in³
sheet density
Cell Length 0.700 - 1.60 mm
0.0276 - 0.0630 in