Zoltek Panex 35® Unsized Chopped Fiber Flake

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 35®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 35® Unsized Chopped Fiber Flake.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unsized Chopped Fiber FlakeApplications include: Carbon papers, infrastructure, full fiber dispersion
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium <= 0.50 %
<= 0.50 %
Component Elements Properties Metric English Comments
Carbon, C 95 %
95 %
Descriptive Properties Value Comments
Fiber Length, mm 13
25
3
6
Sizing Chemistry None