Zoltek Panex 35® Uni-Directional Carbon Fiber Prepreg

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer Zoltek
Trade Name Panex 35®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 35® Uni-Directional Carbon Fiber Prepreg.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uni-Directional Carbon Fiber Prepreg. Several epoxy resins are available for processing flexibility and meet application requirements; resin content 28-45%.Applications include: Wind energy, automotive, petroleum production, aviation, marine, industrial, medical, other transportation, sports
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1904 MPa
276200 psi
Modulus of Elasticity 134 GPa
19400 ksi
Descriptive Properties Value Comments
Areal Weights, g/m2 150 - 900
Roll Length, m 1500
Width, mm 1270