Zoltek Panex 35® Type 85 Chopped Carbon Fiber for High-Temperature Thermoplastics

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 35®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 35® Type 85 Chopped Carbon Fiber for High-Temperature Thermoplastics.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chopped Carbon Fiber for High-Temperature ThermoplasticsApplications include: High temperature environments where chemical resistance, electrical properties, heat aging, dimensional capability, and mechanical properties are required.
Physical Properties Metric English Comments
Bulk Density >= 0.350 g/cc
>= 0.0126 lb/in³
Unpacked Bulk Density
Moisture Absorption at Equilibrium <= 0.20 %
<= 0.20 %
Component Elements Properties Metric English Comments
Carbon, C 95 %
95 %
Descriptive Properties Value Comments
Fiber Length, mm 6
Recommended Thermoplastic Use PAI
PEEK
PEI
PES
PPA
PPS
PSU
Sizing Chemistry Polyimide (PI)
Sizing Content, by weight % 2.75