Zoltek Panex 35® Type 48 Chopped Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 35®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 35® Type 48 Chopped Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chopped Carbon FiberApplications include: RFI/EMI shielding, mechanical wear resistance, weight reduction & dimensional stability
Physical Properties Metric English Comments
Bulk Density >= 0.200 g/cc
>= 0.00723 lb/in³
Unpacked Bulk Density
Moisture Absorption at Equilibrium <= 0.30 %
<= 0.30 %
Component Elements Properties Metric English Comments
Carbon, C 95 %
95 %
Descriptive Properties Value Comments
Compression Ratio, minimum 0.5
Fiber Length, mm 8
Recommended Thermoplastic Use mPPO
PA
PA66
PBT
PET
Sizing Chemistry Polyester
Sizing Content, by weight % 7.5