Zoltek Panex 30® High Purity Carbon Scrim Fabric

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 30®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 30® High Purity Carbon Scrim Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Purity Carbon Scrim FabricApplications include: Lightweight Secondary Reinforcement
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
Component Elements Properties Metric English Comments
Carbon, C 99 %
99 %
Descriptive Properties Value Comments
Areal Weights, g/m2 132
142
44
68
88
Construction Plain Leno Weave
Roll Width, cm 100
Yarn Input 2/10