Zircar Zirconia ZYK-15 Zirconia Cloth Insulation

Category Ceramic , Machinable Ceramic , Oxide , Zirconium Oxide
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Zirconia ZYK-15 Zirconia Cloth Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexible form and provides the lowest thermal conductivity of any commercially available refractory fiber material. ZYK-15 cloth is ideal for temperatures up to 2200°C. The melting temperature is 2590°C. It is suitable for applications such as high energy battery separators, thermal insulation in crystal growing furnaces, and for the filtration of hot gases.ZYK-15 is a true textile constructed of essentially continuous individual filaments fabricated in a tricot knit form. It requires neither binders nor supporting wires in its construction and will comply somewhat to both tensile and compressive forces due to the mechanical interlocking of their fibers. Elongation of 4 to 8% before breaking allows ZYK-15 to conform to irregular surfaces. ZYK-15 can be compressed up to two-thirds of its normal thickness and still recover a major fraction of its original dimension with little fiber damage.The fine capillary and pore structure of ZYK-15, in combination with the hydrophilic nature of zirconia and the serrated surface of the individual fibers in the knit threads, impart excellent wetting solution retention and wicking characteristics to this material.Features: Low Thermal ConductivityHigh PurityExtreme High Temperature StabilityFibers Stabilized with ~10 wt% YttriaCan be Cemented with Zircar Zirconia Cement Type ZR-CEMCan be Rigidized with Zircar Zirconia Rigidizer Type ZR-RIGEasily Cut to SizeAvailable ‘off the shelf’Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Bulk Density 0.680 g/cc
0.0246 lb/in³
Porosity 85 %
85 %
Bulk
Thickness 305 microns
12.0 mil
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 0.544 J/g-°C

@Temperature 93.3 °C
0.130 BTU/lb-°F

@Temperature 200 °F
0.753 J/g-°C

@Temperature 2370 °C
0.180 BTU/lb-°F

@Temperature 4298 °F
Melting Point 2590 °C
4690 °F
Maximum Service Temperature, Air 2200 °C
3990 °F
Continuous
Shrinkage 4.30 %

@Temperature 899 °C,
Time 3600 sec
4.30 %

@Temperature 1650 °F,
Time 1.00 hour
1 hour isothermal soak at 1650°F
Component Elements Properties Metric English Comments
HfO2 1.0 - 2.0 %
1.0 - 2.0 %
Y2O3 10 %
10 %
ZrO2 88 - 89 %
88 - 89 %
Descriptive Properties Value Comments
Tensile Strength per Unit Width 166 gram/cm width
Trace Impurities <0.25%
Weight Per Area 207 g/m2