Material Notes:
ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high temperature applications up to 1260°C (2300°F). Commonly used in the molten metal casting and heat treating industries, ZRCI materials are also used as specialty gasketing in the fuel cell, nuclear, glass and electronic industries, as well as many other applications which require high temperature stability and low thermal conductivity. They also offer excellent corrosion resistance and unique handling strength for easy die-cutting, wrapping and forming.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 0.0900 g/cc
0.00325 lb/in³
Filament Diameter 3.0 - 5.0 µm
3.0 - 5.0 µm
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.0350 MPa
5.08 psi
Thermal Properties Metric English Comments
Melting Point >= 1500 °C
>= 2730 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage 2.10 %

@Temperature 760 °C,
Time 86400 sec
2.10 %

@Temperature 1400 °F,
Time 24.0 hour
2.80 %

@Temperature 1100 °C,
Time 86400 sec
2.80 %

@Temperature 2010 °F,
Time 24.0 hour
6.00 %

@Temperature 1300 °C,
Time 86400 sec
6.00 %

@Temperature 2370 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
MgO 19 - 26 %
19 - 26 %
Other 0.00 - 4.0 %
0.00 - 4.0 %
SiO2 72 - 77 %
72 - 77 %
Descriptive Properties Value Comments
Color Bluish White