Material Notes:
Zetpol 2020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.For seals, rolls, belts, and oil field components. Provides excellent balance between static heat resistance and dynamic hysteresis. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number 24.2 - 31.8
24.2 - 31.8
mg/100mg; ZCI-T-004
Mooney Viscosity 71 - 85

@Temperature 100 °C
71 - 85

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 75
67 - 75
ZCI-T-009
Tensile Strength at Break 20.0 - 30.0 MPa
2900 - 4350 psi
ZCI-T-008
Elongation at Break 400 - 500 %
400 - 500 %
ZCI-T-008
300% Modulus 0.01250 - 0.01650 GPa
1.813 - 2.393 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 91
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 0.5