Material Notes:
Nipol DN 508SCR is a 70/30 fully-fluxed polyblend of medium-high acrylonitrile content.Improved ozone resistance and physical property version of P-70.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Mooney Viscosity 40 - 50

@Temperature 100 °C
40 - 50

@Temperature 212 °F
(1+4)
Ash <= 0.80 %
<= 0.80 %
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 24-27
Heat Loss (%) Max 1
NBR/PVC Ratio 70/30
Type PB