Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Nipol® DN401LL Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® DN401LL Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol DN401LL is a copolymer of butadiene and acrylonitrile whereby, the extremely low acrylonitrile content is designed for the maximum in low temperature performance. Sufficient antioxidant is added during manufacture for normal storage conditions.Very good low-temperature flexibility and low viscosity for superior processing properties.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Mooney Viscosity 32 - 44

@Temperature 100 °C
32 - 44

@Temperature 212 °F
(1+4)
Ash <= 0.70 %
<= 0.70 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 17-20
Heat Loss (%) Max 0.5
Hot/Cold C
Users viewing this material also viewed the following: