Zeon Chemicals Nipol® 33-5SR Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 33-5SR Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Special-purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.Special purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Mooney Viscosity 41 - 51

@Temperature 100 °C
41 - 51

@Temperature 212 °F
(1+4)
Ash <= 0.75 %
<= 0.75 %
T-4410
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 32-34
Heat Loss (%) Max 0.5
Hot/Cold C