Zeon Chemicals Nipol® 1001LG Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1001LG Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol 1001LG is a copolymer of butadiene and acrylonitrile with very high oil resistance. Its properties are similar to those of Nipol 1001CG with the exception that: a) nomilling is required for ungelled cements; and b) non-polymer constituents have been designed so as not to interfere with adhesion. Sufficient antioxidant is added during manufacture for normal storage conditions. No fatty acid or fatty soap is used in the manufacturing process for this product.Similar to 1001CG, but can be dissolved in solvents without milling. Contains no fatty acids or soaps.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Viscosity 1000 - 10000 cP
1000 - 10000 cP
Unmilled Cement; Zeon Test #328
Mooney Viscosity 70 - 90

@Temperature 100 °C
70 - 90

@Temperature 212 °F
(1+4)
Ash <= 0.40 %
<= 0.40 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 39-42
Heat Loss (%) Max 0.5
Hot/Cold H