Hydrin H1100 is an epichlorohydrin/allyl glycidyl ether copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin H1100 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Hydrin H copolymerized with AGE for sulfur or peroxide vulcanization. Excellent resistance to permeation by gases.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Mooney Viscosity 48 - 68

@Temperature 100 °C
48 - 68

@Temperature 212 °F
(1+4)
Ash <= 1.0 %
<= 1.0 %
Zeon Test #1358
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -26.0 °C
-14.8 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361
Descriptive Properties Value Comments
AGE Content, % 6.7-8.7