Zeon Chemicals HyTemp® ZC-50 Polyacrylate Curative

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® ZC-50 Polyacrylate Curative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp ZC-50 is a Zisnet-F based - cure package dispersion for use in curing chlorine functional, acrylic polymers. Fast cure rates and excellent scorch-safety at 125°C make it particularly useful for injection molding type compounds. The dispersion is in the form of orange slabs dusted with clay and free from foreign materials.Fast cure package for HyTemp AR70 series. (50% active)
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Component Elements Properties Metric English Comments
Nitrogen, N 3.0 - 5.6 %
3.0 - 5.6 %