Zeon Chemicals HyTemp® 4454 AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® 4454 AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp 4454 is a ground form of HyTemp 4054, which contains one or more acrylic esters with a small percentage of a carboxy/chlorine cure site.Particulate version of HyTemp 4054.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 22 - 34

@Temperature 100 °C
22 - 34

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.60 %
<= 0.60 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -41.0 °C
-41.8 °F
Gehman T100
Glass Transition Temp, Tg -40.6 - -31.7 °C
-41.1 - -25.1 °F
Zeon Test #1273
Descriptive Properties Value Comments
% Volume Swell 63
Curesite Dual
Gel-Mek (%), max 20
Heat Loss (%) Max 0.5