Zeon Chemicals HyTemp® 4451CG AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® 4451CG AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Particulate version of HyTemp 4051CG. Suitable for adhesives, caulks, sealants, and binders.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Gehman T100
Descriptive Properties Value Comments
% Volume Swell 11
Curesite Dual