Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals HyTemp® 4052EP AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® 4052EP AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp 4052EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance with good low temperature.Easy processing version of HyTemp 4052.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 20 - 35

@Temperature 100 °C
20 - 35

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.50 %
<= 0.50 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -32.0 °C
-25.6 °F
Gehman T100
Glass Transition Temp, Tg -33.1 - -25.2 °C
-27.6 - -13.4 °F
Descriptive Properties Value Comments
% Volume Swell 17
Curesite Dual
Gel-Mek (%), max 15
Heat Loss (%) Max 0.7