Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Unreinforced
Manufacturer Zell-Metall Engineering Plastics
Trade Name Zellamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads for rolling mills.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Dry Density
Moisture Absorption at Equilibrium 2.5 - 3.0 %
2.5 - 3.0 %
Saturation at 50% RH
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 76 - 78
76 - 78
DIN 53505
Tensile Strength at Break 63.0 - 65.0 MPa
9140 - 9430 psi
DIN 53455
Elongation at Break 100 - 150 %
100 - 150 %
DIN 53455
Tensile Modulus 2.00 GPa
290 ksi
DIN 53457
0.300 GPa

@Temperature 100 °C
43.5 ksi

@Temperature 212 °F
DIN 53457
Charpy Impact, Notched 6.00 - 12.0 J/cm²
28.6 - 57.1 ft-lb/in²
DIN 53453
Coefficient of Friction 0.050 - 0.10
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Tensile Creep Modulus, 1000 hours <= 450 MPa
<= 65300 psi
DIN 53444
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.67 J/g-°C
0.399 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 205 °C
401 °F
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long time operation
120 - 140 °C
248 - 284 °F
medium time operation
160 °C
320 °F
a few hours operation
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+12 - 5.00e+12 ohm-cm
3.00e+12 - 5.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+10 - 3.00e+10 ohm
1.00e+10 - 3.00e+10 ohm
DIN 53482
Dielectric Constant 12

@Frequency 1e+6 Hz
12

@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
DIN 53481
Dissipation Factor 0.15

@Frequency 1e+6 Hz
0.15

@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 V
600 V
KV Method; DIN 53480
Descriptive Properties Value Comments
Permissible Unit Pressure 25 - 30 MPa
Time yield limit up to 8
s1/1000; DIN.53444
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved