Material Notes:
Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo material. Zelfo is an economic, adaptable and sustainable alternative to wood, plastics, and other materials for 2D and 3D applications.Product Design & Built Environment/Construction: Uses across consumer products, packaging, interior design, and construction include housings, furniture, flooring, and paneling. Grade HZ is based on hemp cellulose.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Tensile Modulus 6.55 GPa
950 ksi
Flexural Strength 95.0 MPa
13800 psi
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
Underground specimens
Izod Impact, Unnotched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
Underground specimens