Zelfo Technology Zelfo® HG Cellulose Fiber Material

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic
Manufacturer Zelfo Technology
Trade Name Zelfo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zelfo Technology Zelfo® HG Cellulose Fiber Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo material. Zelfo is an economic, adaptable and sustainable alternative to wood, plastics, and other materials for 2D and 3D applications.Product Design & Built Environment/Construction: Uses across consumer products, packaging, interior design, and construction include housings, furniture, flooring, and paneling. Grade HG is based on hemp.
Physical Properties Metric English Comments
Density 0.500 g/cc
0.0181 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.00 MPa
1020 psi
Tensile Modulus 1.50 GPa
218 ksi
Flexural Strength 17.0 MPa
2470 psi
Izod Impact, Notched (ISO) 1.00 kJ/m²
0.476 ft-lb/in²
Izod Impact, Unnotched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²