Wingate Alloys Winco XR Special High Strength Alloy Wear Bar

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Wingate Alloys
Trade Name Winco
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wingate Alloys Winco XR Special High Strength Alloy Wear Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A superior substitute for 8620, 4140, 4130 and 6150.Winco XR Special’s high physical properties and the fact that it can be heat treated by use of several different methods, resulting in different ranges of hardness, make it the perfect choice as a long lasting steel in may applications. Advantages:Pre-hardened steel with hardness range for many tool room and maintenance applications.Can be re-hardened to various hardness ranges by flame hardening, carburizing, nitriding or through hardening to a higher hardness range.All melts of Winco XR Special are electric furnace, vacuum degassed to provide optimum cleanliness of the finished product.High impact and wear properties retained at weld joints. Information from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28 - 32
28 - 32
55 - 57
55 - 57
Re-hardened
Component Elements Properties Metric English Comments
Carbon, C 0.35 %
0.35 %
Chromium, Cr 0.85 %
0.85 %
Iron, Fe >= 96.9 %
>= 96.9 %
Manganese, Mn 0.75 %
0.75 %
Molybdenum, Mo 0.45 %
0.45 %
Silicon, Si 0.25 %
0.25 %
Tungsten, W 0.45 %
0.45 %