Wingate Alloys Winco Tong Bits for Steel, Alloy, Stainless and Aluminum Plate and Billet Handling

Category Metal , Ferrous Metal , Alloy Steel , Stainless Steel
Manufacturer Wingate Alloys
Trade Name Winco
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wingate Alloys Winco Tong Bits for Steel, Alloy, Stainless and Aluminum Plate and Billet Handling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For longer wear life, less downtimeWinco Tong Bits are made of a proprietary Winco HM-3 Alloy used on the end of cranes for gripping and moving slabs and billets of all varieties of steel grades.Advantages:Manufactured to customer OEM specifications.Material and machining cost savings.Less downtime for replacement.Longer wear life.Information from Wingate Alloys Inc.
Component Elements Properties Metric English Comments
Carbon, C 0.30 - 0.42 %
0.30 - 0.42 %
Chromium, Cr 4.75 - 5.75 %
4.75 - 5.75 %
Iron, Fe 87.58 - 89.7 %
87.58 - 89.7 %
Manganese, Mn 0.75 %
0.75 %
Molybdenum, Mo 1.25 - 1.75 %
1.25 - 1.75 %
Nickel, Ni 1.0 %
1.0 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si 1.5 %
1.5 %
Sulfur, S <= 0.025 %
<= 0.025 %
Vanadium, V 0.75 - 1.2 %
0.75 - 1.2 %