Material Notes:
Nicro-45 air hardened, high alloy steel is intended specifically for applications requiring a high degree of abrasion and wear resistance.Unlike normal quenched and tempered material, high-heat cycling with air-cooling alone will not result in loss of hardenability and wear resistance. Used by industries such as mining, forestry, quarrying and construction. Nicro 45 is the cost-effective choice for parts subjected to extremely high levels of wear.Information from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Brinell 420 - 465
420 - 465
Tensile Strength 1450 MPa
210000 psi
Tensile Strength, Yield 1250 MPa
181000 psi
Elongation at Break 11.5 %
11.5 %
2[in]
Component Elements Properties Metric English Comments
Boron, B 0.0040 %
0.0040 %
Carbon, C 0.25 %
0.25 %
Chromium, Cr 1.6 %
1.6 %
Iron, Fe 92.916 %
92.916 %
Manganese, Mn 1.0 %
1.0 %
Molybdenum, Mo 0.35 %
0.35 %
Nickel, Ni 3.5 %
3.5 %
Phosphorous, P 0.30 %
0.30 %
Silicon, Si 0.35 %
0.35 %