Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 15.7 g/cc
0.567 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 255 MPa
37000 psi
Thermal Properties Metric English Comments
CTE, linear 12.3 µm/m-°C

@Temperature 20.0 °C
6.83 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 27.0 W/m-K
187 BTU-in/hr-ft²-°F
Melting Point 363 °C
685 °F
Solidus 363 °C
685 °F
Liquidus 363 °C
685 °F
Component Elements Properties Metric English Comments
Gold, Au 96.85 %
96.85 %
Silicon, Si 3.15 %
3.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000372 ohm-cm
0.00000372 ohm-cm