Wieland 1932 Wilaform Palladium

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1932 Wilaform Palladium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal use palladium alloy with beautiful grey color and noble gloss.Applications: casting, chains, laminar decoration, tubingDental
Physical Properties Metric English Comments
Density 12.0 g/cc
0.434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 130
130
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 1550 - 1650 °C
2820 - 3000 °F
Solidus 1550 °C
2820 °F
Liquidus 1650 °C
3000 °F
Component Elements Properties Metric English Comments
Palladium, Pd 95 %
95 %
Ruthenium, Ru 5.0 %
5.0 %
Descriptive Properties Value Comments
Color grey