Wico Plast Wicotal 25 Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Wico Plast
Trade Name Wicotal
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wico Plast Wicotal 25 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsExtrusionAll information provided by Wico Plast, Warenhandelsges. mbH
Physical Properties Metric English Comments
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
DIN 53455/ISO 527
Tensile Modulus 2.75 GPa
399 ksi
DIN 53457/ISO 527
Izod Impact, Unnotched (ISO) NB
NB
DIN 53453