Wico Plast Wicoran 27 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Wico Plast
Trade Name Wicoran
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wico Plast Wicoran 27 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsInjection moldingGalvanoAll information provided by Wico Plast, Warenhandelsges. mbH
Physical Properties Metric English Comments
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Izod Impact, Unnotched 2.45 J/cm
4.59 ft-lb/in
ASTM D256