Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental)

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Westlake Chemical Corporation
Trade Name Tymax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake GA7501 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications where more heat resistance is required than typical acrylate polymers provide. Westlake GA7501 is designed to tie polyethylene or polyester to resins that typically have poor bonding characteristics such as polyamide and EVOH. This polymer can also be used as a compatibilizer for compounding dissimilar resins. Its applications include: tie-layers, packaging, and compounding.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
Methyl Acrylate Content 20 %
20 %
Westlake
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
DSC; ASTM D3418
Vicat Softening Point 43.0 °C
109 °F
ASTM D3418