Westlake Plastics Propylux® Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Westlake Plastics
Trade Name Propylux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Propylux® Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable for various applications. Propylux Natural, Void Free, and 944 are FDA compliant.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.9 MPa
5200 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Tensile Modulus 1.65 GPa
240 ksi
ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 146 µm/m-°C

@Temperature 20.0 °C
81.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 166 °C
330 °F
ASTM D4591
Maximum Service Temperature, Air 82.2 °C
180 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149