Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Propylux® CN-F Polypropylene (conductive)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Carbon Fiber Filled
Manufacturer Westlake Plastics
Trade Name Propylux® CN-F
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Propylux® CN-F Polypropylene (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined and fabricated, and has good overall mechanical properties.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Water Absorption 0.010 %
0.010 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B