Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Steel Filled
Manufacturer Westlake Plastics
Trade Name Pomalux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an excellent choice for situations where carbon-based conductive fillers are not acceptable. Easily machined with carbide-tipped tooling to tight tolerances. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength, Yield 59.3 MPa
8600 psi
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 88.2 µm/m-°C

@Temperature 20.0 °C
49.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257
Users viewing this material also viewed the following: