Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Westlake Plastics
Trade Name Crystat®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Crystat® ABS (anti-static).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semitransparent, inherently anti-static material available in roll stock or thin gauge sheet. Its strength and clarity make it excellent for thermoforming.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.3 MPa
5700 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Strength 60.7 MPa
8800 psi
ASTM D790
Flexural Modulus 1.775 GPa
257.5 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 3.00e+11 ohm
3.00e+11 ohm
Dry; ASTM D257