Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Westlake Plastics
Trade Name Absylux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in thinner gauges, and is bondable with WELDON® 1707.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Water Absorption 1.7 %
1.7 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 13 %
13 %
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 - 1.00e+11 ohm-cm
1.00e+9 - 1.00e+11 ohm-cm
Dry; ASTM D257
Surface Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Dry; ASTM D257
Static Decay <= 0.30 sec
<= 0.30 sec
15% RH; MIL-B-81705-B