Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Westlake Plastics
Trade Name Absylux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D7852
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Yield Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 4.11 J/cm
7.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0580 in
Copyright © lookpolymers.com All Rights Reserved