Material Notes:
WESTLAKE HIFOR Xtreme Polyethylene SC74836 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock and processing aid. Films produced with this resin exhibit extreme toughness, with excellent gloss and clarity for a product of this density. Features of this resin include high stiffness and high ultimate tensile strength.Application/UsesFresh produce packagingFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.60 g/10 min
0.60 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 750 %
750 %
ASTM D882
Film Elongation at Break, TD 1150 %
1150 %
ASTM D882
Dart Drop 5.91 g/micron
150 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Film Tensile Strength at Break, TD 43.4 MPa
6300 psi
ASTM D882
1% Secant Modulus, MD 248 MPa
36000 psi
ASTM D882
1% Secant Modulus, TD 317 MPa
46000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 60 %
60 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 204 - 216 °C
400 - 420 °F
Blow-up Ratio (BUR) 2.4
2.4
Descriptive Properties Value Comments
Process Blown Film
Film
Region US & Canada
Bamberger Polymers Distribution