Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® E-16 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water resistance, low color, and consistent quality through SPC methods. Their applications include: PVC lubricants, textile softener/lubricant, floor polish, plastic additive applications, paper coating lubricant, fruit coating, agricultural sprays, car polish, and fiberglass sizing. Products are supplied as free flowing pellets; although some products may be available in powder form. Products made with these polymers will have attributes that deliver: abrasion resistance, moisture and grease resistance, surface slip and release properties, and compatibility with other polymers, pigments, and fillers.
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM-D5
Brookfield Viscosity 500 cP

@Temperature 140 °C
500 cP

@Temperature 284 °F
Thermosel; ASTM-D3226
700 cP

@Temperature 125 °C
700 cP

@Temperature 257 °F
Thermosel; ASTM-D3226
Molecular Weight 1037 g/mol
1037 g/mol
M<sub>n</sub>
4538 g/mol
4538 g/mol
M<sub>w</sub>
Thermal Properties Metric English Comments
Ring & Ball Softening Point 102 °C
216 °F
ASTM-E28
Optical Properties Metric English Comments
Gardner Color Number 1.0
1.0
ASTM-D1544
Chemical Properties Metric English Comments
Total Acid Number 17
17
ASTM-D1386
Descriptive Properties Value Comments
Penetration Hardness 4 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm