Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name Elevate™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake Elevate™ EF526 resin is a 16% EVA copolymer designed for cast film, extrusion coatings, and thermal laminations.Application/UsesThermal laminationsCast FilmExtrusion CoatingsThis resin grade complies with 21 CFR, section 177.1350.
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Vinyl Acetate Content 16 %
16 %
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
15s; ASTM D2240
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Elongation at Break 590 %
590 %
ASTM D638
Flexural Modulus, 1% Secant 62.1 MPa
9000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 79.0 °C
174 °F
Peak; Westlake Method
Vicat Softening Point 65.0 °C
149 °F
ASTM D1525
Descriptive Properties Value Comments
Process Coating
Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: