Westlake EMAC® Plus SP1307 20% Ethylene-Methyl Acrylate Copolymer

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer Westlake Chemical Corporation
Trade Name EMAC® Plus
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® Plus SP1307 20% Ethylene-Methyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake EMAC® Plus SP1307 is a 20% EMA copolymer designed for extrusion coating, laminations, and blending where EMA properties are needed, but higher temperature resistance is required. SP1307 is compatible with and provides increased adhesion to polyolefins, polyesters, and other polymers as a tie-layer, non-skid coating, or heat seal layer. The higher melting point of this EMAC® Plus grade offers EMA performance with improved heat resistance.Applications: films, disposable gloves, and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Methyl Acrylate Content 20 %
20 %
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 825 %
825 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
by DSC; ASTM D3418
Vicat Softening Point 46.0 °C
115 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating
Extrusion
Region US & Canada