WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipment to produce molded items with excellent gloss, clarity and warpage resistance.Application/UsesMedicalFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.00 MPa
870 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 100 %
100 %
500mm/min; ASTM D638 Type IV Specimen
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Injection Molding