Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake 1230S PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake 1230S PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake PVC 1230S resin is a medium molecular weight homopolymer designed primarily for the extrusion of rigid products.Information provided by Westlake Chemical Corporation
Physical Properties Metric English Comments
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Particle Mesh Size 40 Mesh
40 Mesh
99.9% min; ASTM D1921
200 Mesh
200 Mesh
4.0% max; ASTM D1921
Viscosity Measurement 0.90
0.90
Inherent; ASTM D5225
2.2

@Temperature 25.0 °C
2.2

@Temperature 77.0 °F
Relative (1.0% in Cyclohexanone)
Collected Volatile Condensable Material <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
K-Value 66
Users viewing this material also viewed the following: