Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellpet® PR109-N1 Unfilled PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellpet®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellpet® PR109-N1 Unfilled PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unfilled PETInformation provided by Wellman.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183-87
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm
0.0010 - 0.0050 in/in
ISO DIS 294-4
Melt Flow 3.5 g/10 min

@Load 0.325 kg,
Temperature 280 °C
3.5 g/10 min

@Load 0.716 lb,
Temperature 536 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
ASTM D-2240
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527-93
Elongation at Break 250 %
250 %
ISO 527-93
Flexural Strength 60.0 MPa
8700 psi
ISO 178-93
Flexural Modulus 2.70 GPa
392 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-93
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D-2240
Transmission, Visible 87 %
87 %
ASTM D-1003
Users viewing this material also viewed the following: