Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellpet® MRGF101-GY1 PET, 29% Mineral/Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellpet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellpet® MRGF101-GY1 PET, 29% Mineral/Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183-87
Linear Mold Shrinkage 0.0075 - 0.0095 cm/cm
0.0075 - 0.0095 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 95.0 MPa
13800 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Yield Strength 130 MPa
18900 psi
ISO 178-93
Flexural Modulus 8.00 GPa
1160 ksi
ISO 178-93
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 250 °C
482 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-93